Mo-Cu Alloy Rod
Mo-Cu Alloy Rod

Mo-Cu Alloy Rod

Mo-Cu Alloy rod is the material of choice for devices such as heat sinks, microelectronic components and aerospace accessories. The most typical molybdenum-copper ratios are 70/30 and 80/20. Generally, the ratios from Mo90Cu10 to Mo60Cu40 can be produced by our company.
Send Inquiry

Description of Mo-Cu Alloy Rod

 

Molybdenum-copper material, like tungsten-copper material, is a pseudo-alloy composed of two mutually immiscible metal phases. Therefore, this material should have the characteristics of both constituent metals, and can learn from each other to obtain good comprehensive performance.

Mo-Cu Alloy rod combines the high thermal conductivity of copper and the low thermal expansion of molybdenum. The most typical molybdenum-copper ratios are 70/30 and 80/20. Generally, the ratios from Mo90Cu10 to Mo60Cu40 can be produced by our company.

 

Mo-Cu Alloy rod has many advantages, such as high electrical and thermal conductivity, convenient processing, good plasticity, good high-temperature stability, and excellent arc ablation resistance.


Mo-Cu Alloy rod is the material of choice for devices such as heat sinks, microelectronic components, and aerospace accessories. In the actual application process, by adjusting the range of composite ratio, the thermal expansion coefficient of molybdenum-copper alloy components, such as radiators and radiators can be matched with those of other device components, and the internal thermal stress can be reduced to significantly improve the performance of the device. functionality and reliability.

 

Manufacturing Process of Mo-Cu Alloy Rod


Smelting: Isostatic pressing (high-temperature sintering-copper infiltration) is adopted.
Processing: After turning, the surface shall not have defects such as holes, cracks, delamination or inclusions.
Heat treatment: Hot forging deformation, when the deformation is less than 60%, the relative density and uniformity of the rod are improved.

 

Specification of Mo-Cu Alloy Rod

 

Grade

MoCu20, MoCu30, MoCu25, MoCu15

Chemical Composition

Molybdenum 70%-90%, Copper 10%-30%

Process

Isostatic pressing, Annealing, Rolling, Sintering, Skeleton melting method

Diameter

30 mm-100mm

Length

3-2000mm

Density

≥9.3-9.91g/cm3

Conductivity

30%-50%IACS

Surface

Polishing, Pickling, Grinding

Shape

Round

Standard

ASTM, GB

 

Testing and Quality Control of Mo-Cu Alloy Rod

 

Dimensional accuracy: diameter tolerance ±0.5 mm (10<Φ≤25 mm), length tolerance ±5 mm (100<Φ≤200 mm).
Nondestructive testing: 100% eddy current testing (ET) + ultrasonic flaw detection (UT) to ensure no cracks and inclusions.
Surface quality: smooth surface, no oxidation color, no cracks, peeling, burrs, spots and inclusions, etc.

 

product-760-700

 

FAQ for Mo-Cu Alloy Rod

 

Are you a Mo-Cu Alloy Rod factory or a Mo-Cu Alloy Rod manufacturer?
A: Yes, we are a Mo-Cu Alloy Rod factory, but we generally use our trading company to handle the business abroad. It will be more convenient to receive the remittance and arrange the shipment.

What is the delivery method of Mo-Cu Alloy Rod?
A: Generally, we send Mo-Cu Alloy Rod by UPS, DHL, or FedEx. Also, we can send by sea to a seaport or by air to the closest airport.

Why is your Mo-Cu Alloy Rod so cost-effective?
A: We cut out the middlemen in the end-to-end manufacturing process, and we obtain raw material directly from its source.

Do you do spot quality inspection of Mo-Cu Alloy Rod or full inspection of Mo-Cu Alloy Rod?
A: 100% full inspection for sure. All unqualified Mo-Cu Alloy rods are discarded.

How do you ensure your lead time for Mo-Cu Alloy Rod?
A: From material preparation to machining and finally to a full inspection. Every stage of production is strictly monitored and controlled to give you an accurate delivery time.

What is the MOQ of Mo-Cu Alloy Rod?
A: Depends on the quantity of Mo-Cu Alloy Rod; generally, no MOQ limit.

How to pay for Mo-Cu Alloy Rod?
A: A bank transfer (T/T) will be acceptable.

What is the delivery time of Mo-Cu Alloy Rod?
A: Around 7-20 days, which depends on the quantity and production of Mo-Cu Alloy Rod.

What kind of package of Mo-Cu Alloy Rod is it?
A: Generally, we use a carton case or a plywood case with protective material inside to ensure the safety of the Mo-Cu Alloy Rod.

What is the lead time of Mo-Cu Alloy Rod?
A: From the order placed to cargo receiving will take around 10-25 days.

 

product-700-700

 

Picture of Mo-Cu Alloy rod

 

product-700-700

Hot Tags: mo-cu alloy rod, China mo-cu alloy rod suppliers, factory, Tungsten Cemented Carbide Nozzles, Kovar Seamless Pipe, Zirconium 702 Pipe, Rectangular Neodymium Pot Magnet, Inconel 625 Pipe, Beryllium Copper Wire